SC 14.4v 2400mah qayta zaryadlanuvchi nim batareya
Mahsulot nomi | AA 2500mah 1.2V NI-MH qayta zaryadlanuvchi quvvat batareyasi |
Hajmi | AA |
Imkoniyatlar | 2500mAh |
Kuchlanish | 1.2V |
Kimyoviy tizim | Nikel-metal gidridli batareya |
Sikl hayoti | 500-1000 marta |
Kurtka | PVX |
Sertifikatlar | Idoralar ROHS SGS MSDS |
Standart zaryadlash oqimi | 16 soat davomida 0,1A |
Standart tushirish oqimi | 0,2A |
Zaryadlash harorati | 0 dan 45 darajagacha bo'lgan harorat |
Bo'shatish harorati | -20 dan 60 darajagacha |
Sinovlar tovarlarni qabul qilinganidan keyin bir oy ichida quyidagi shartlar asosida o'tkazilishi kerak.
Sinov sharti:
Harorat: 20 ± 5 ℃
Nisbiy namlik: 65 ± 20%
Atmosfera bosimi: 86 ~ 106kPa
Zaryadni tushirishning standart tavsifi
Bo'shatish: 6000mA (1C) dan 12.0V gacha
Zaryad: 6000mA (1C) × 1 soat , 1200mA (0.2C) × 1 soat
Bo'shatish: 6000mA (1C) dan 12.0V gacha
Yo'q | Sinov | Birlik | Ta'rif | Ahvoli | Eslatma |
1 | Ochiq elektron zo'riqishida | V | ≥15 | Zaryad olgandan keyin 1 soat ichida | |
2 | Ichki qarshilik | mΩ | ≤32 | 50% SOC | |
3 | Ichki empedans | mΩ | ≤13.8 | 1 kHz | |
4 | O'z-o'zidan tushirish tezligi | % | < 18 | 55 ± 2 ℃ dam olish 3 kun, 20 ± 2 ℃ dam olish 7 kun | |
5 | Energiya samaradorligi | % | ≥85 | 25 ℃ | |
6 | Volumetrik samaradorlik | % | > 95 | 25 ℃ | |
7 | Sikl hayoti | Hafta | > 3000 | 80% DOD | 90% to'lash, 10% to'lash |
Yo'q. | Batareya parametrlari | Sinov usuli | Standart |
1 | Tashqi ko'rinishi | Yaxshi yorug'lik sharoitida batareyaning ko'rinishini vizual ravishda tekshiring. | To'g'ri tartiblangan, ishonchli va aniq belgilangan. Yoriqlar va izlardan ozod. |
2 | Vibratsiyali qarshilik | Batareya modulini tebranish sinov stendiga o'rnatdi, quyidagi shartlarga muvofiq chiziqli skrining tebranish sinovini o'tkazing: - Tebranish yo'nalishi: yuqoriga va pastga bitta tebranish; - Vibratsiyali chastotasi: 10 Gts ~ 55 Gts; - Max tezlashishi: 30m / s2; - Tebranish vaqti: 3s | Hech qanday deformatsiya va oqish yo'q |
3 | Ortiqcha zaryadsizlanish sinovi | 1. Zaryadlashning standart usuliga muvofiq; 2. 6A oqimi bilan zaryadsizlantirish (Agar elektron himoya chizig'i mavjud bo'lsa, tushirish elektron himoya chizig'i vaqtincha olib tashlanadi) tushirish 90min; 1 soatni kuzating. | Hech qanday portlash, yong'in yoki oqish yo'q. |
4 | Ortiqcha quvvat sinovi | 1. standart zaryadlash usuli bilan zaryadlash; 2. 6A oqimi bilan 1H zaryadlang; 3. 1 soatga rioya qiling. | Portlash yoki yong'in yo'q. |
5 | Qisqa tutashuv sinovi | 1. standart zaryadlash usuli bilan zaryadlash; 2. Batareyaning tashqi qisqa tutashuvi 10 min, tashqi chiziqqa qarshilik esa 5mΩ dan kam bo'lishi kerak; 3. 1 soatga rioya qiling. | Portlash yoki yong'in yo'q. |
6 | Isitish sinovi | 1. standart zaryadlash usuli bilan zaryadlash; 2. Harorat xonasi xona haroratidan 85 + 2 daraja C gacha 5 minut tezlikda isitiladi va 2 soatdan keyin isitish to'xtatiladi; 3. 1 soatga rioya qiling. | Portlash yoki yong'in yo'q. |
7 | Ekstruziya sinovi | 1. standart zaryadlash usuli bilan zaryadlash; 2. Ekstruziya yo'nalishi: batareya monomerining joylashuv yo'nalishiga perpendikulyar ravishda bosim 3. Ekstruziya plitasi shakli: 75 mm yarim tsilindrning radiusi, yarim tsilindrning uzunligi (L) ekstrudirovka qilingan batareyaning hajmidan katta; 4. Ekstruziya tezligi: (5 ± 1) mm / s ; 5. Ekstruziya darajasi: kuchlanish 0V ga etadi yoki deformatsiya miqdori 30% ga, yoki ekstruziya bosimi 200KN ga etadi, keyin ekstruziya qilishni to'xtating; 6. 1 soatga rioya qiling. | Portlash yoki yong'in yo'q. |
8 | Akupunktur sinovi | 1. standart zaryadlash usuli bilan zaryadlash; 2. Diametri 6 mm dan 10 mm gacha bo'lgan yuqori haroratga chidamli po'lat bilan (uchi konusning burchagi 45 darajadan 60 darajaga, silliq sirt, zang bo'lmagan igna, oksid qatlami va moy), 25 + 5mm / s tezlikda, vertikaldan boshlab batareya plitalari yo'nalishi bo'yicha kamida 3 ta monomerni aylantiring; 3. 1 soatga rioya qiling. | Portlash yoki yong'in yo'q. |
Biz bilan bog'lanish Narxlar, qadoqlash.so'lash va chegirmalar haqida ko'proq ma'lumot olish uchun.